View Single Post
  #7  
Old 08-05-2019, 08:07 PM
stephenmarklay stephenmarklay is offline
Senior Member
 
Join Date: Sep 2009
Location: Spokane WA
Posts: 5,021
Quote:
Originally Posted by AngryScientist View Post
dont worry about the hone.

blast the inside of the tubes with a corrosion inhibitor and call it good. most people like framesaver, which is great, but any marine grade corrosion inhibitor works as well. dont sweat surface rust on the inside of tubes, no big deal, especially caught early, like you have. corrosion inhibitor will check the propagation of rust and you're good to go.
I am pretty sure that frame saver IS CRC HD rust inhibitor.
Reply With Quote